The outer edge of this residue corresponded to the just-peeled layer that had been applied on 15 Nov 2019; the inner edge of the residue and some other features corresponded to the voids previously left in first contact application for alignment, a technique which has been used with this optic but which is no longer in use.
The sampling for this single FTIR sample consisted of 3x passes over an area on the left-hand side of the S1 surface of ETM09 measuring about 6" x 3" (18 in^2). GariLynn and Stephen were present in the Downs B119 cleanroom at Caltech.